Rurka termokurczliwa cienkościenna
H-1
- Material: Crosslinked polyolefinnon flame retardant
- Color: black, transparent
- Working temperature: -55°C do 105°C
- Min. shrink temp.: 70ºC
- Min. full shrink temp.: 95ºC
- RoHS Compliant
Part No | Size | Before heat shrink | After hest shrink | Spool | |
---|---|---|---|---|---|
Min. dia. | Max. dia. | Min. wall wthickness | |||
[inch] | [mm] | [m] | |||
H-1-1.2 | 3/64 | 1.2 | 0.50 | 0.33 | 150 |
H-1-1.6 | 1/16 | 1.6 | 0.75 | 0.36 | 150 |
H-1-2.4 | 3/32 | 2.4 | 1.25 | 0.44 | 150 |
H-1-3.2 | 1/8 | 3.2 | 1.50 | 0.44 | 150 |
H-1-4.8 | 3/16 | 4.8 | 2.50 | 0.56 | 75 |
H-1-6.4 | 1/4 | 6.4 | 3.00 | 0.56 | 75 |
H-1-9.5 | 3/8 | 9.5 | 5.00 | 0.56 | 75 |
H-1-12.7 | 1/2 | 12.7 | 6.50 | 0.65 | 50 |
H-1-15.9 | 5/8 | 15.9 | 8.00 | 0.69 | 30 |
H-1-19.1 | 3/4 | 19.1 | 10.00 | 0.80 | 30 |
H-1-25.4 | 1 | 25.4 | 12.00 | 0.90 | 30 |
H-1-31.8 | 1 1/4 | 31.8 | 15.00 | 0.90 | 30 |
H-1-38.1 | 1 1/2 | 38.1 | 20.00 | 1.00 | 30 |
H-1-50.8 | 2 | 50.8 | 25.00 | 1.00 | 30 |
Specyfikacja:
Własności | Test | Wynik testu |
---|---|---|
Temperatura pracy | UL 224 | -55°C do 105°C |
Wytrzymałość | ASTM D 2671 | >12MPa |
Wydłużenie | ASTM D 2671 | 400% |
Skurcz wzdłużny | UL 224 | ±5% |
Mimośrodowość | ASTM D 2671 | <30% |
Starzenie cieplne | 158°C/168 hrs | >11MPa >200% |
Palność | VW-1 | palna |
Oporność skrośna | ASTM D 2671 | >1014Ωcm |
Zachowanie w kontakcie z Cu | ASTM D 2671 | zaliczony |
Korozja Cu | UL 224 | Nie powoduje |